Written by Willy Gerber
|
|
Monday, 16 June 2008 21:07 |
| Metal | Density (kg/m3) | | Aluminium - melted | 2560-2640 | | Aluminium bronze (3-10% Al) | 7700-8700 | | Aluminium foil | 2700-2750 | | Antifriction metal | 9130-10600 | | Beryllium | 1840 | | Beryllium copper | 8100-8250 | | Brass - casting | 8400-8700 | | Brass - rolled and drawn | 8430-8730 | | Bronze - lead | 7700-8700 | | Bronze - phosphorous | 8780-8920 | | Bronze (8-14% Sn) | 7400-8900 | | Cast iron | 6800-7800 | | Cobolt | 8746 | | Copper | 8930 | | Delta metal | 8600 | | Electrum | 8400-8900 | | Gold | 19320 | | Iron | 7850 | | Lead | 11340 | | Light alloy based on Al | 2560-2800 | | Light alloy based on Mg | 1760-1870 | | Magnesium | 1738 | | Mercury | 13593 | | Molybdenum | 10188 | | Monel | 8360-8840 | | Nickel | 8800 | | Nickel silver | 8400-8900 | | Platinum | 21400 | | Plutonium | 19800 | | Silver | 10490 | | Steel - rolled | 7850 | | Steel - stainless | 7480-8000 | | Tin | 7280 | | Titanium | 4500 | | Tungsten | 19600 | | Uranium | 18900 | | Vanadium | 5494 | | White metal | 7100 | | Zinc | 7135 | Copyright gPhysics.net
|